Nanoindentation (single cycle) test data for Model Alloy (Fe-9Cr) material at 23 °C and maximum indenter force of 5.005 mN (thirteenth nominally repeat test)
收藏官方服务:
资源简介:
Data created at the European Commission JRC during the H2020 project on multiscale modeling for fusion and fission materials (M4F), funded from the Euratom research and training programme 2014-2018 under grant agreement No. 755039.
本数据集由欧洲委员会JRC在H2020项目期间创建,该项目聚焦聚变与裂变材料多尺度建模(M4F),由2014-2018年Euratom研究与培训计划资助,资助协议编号为755039。
创建时间:
2020-01-14