遇见数据集

data from: Evaluation of consolidated waterlogged archaeological wood using nanoindentation and ATR-FTIR imaging

收藏
Figshare2021-08-03 更新2026-04-08 收录
官方服务:

资源简介:

The compressed files contain 22 files required by making Figure 3, Figure 5-12 to provide details of the experiments and support the discussion in the paper.

创建时间:
2021-08-03