Data for "High-temperature low-cycle fatigue and fatigue-creep behaviour of Inconel 718 superalloy: Damage and deformation mechanisms"

收藏
NIAID Data Ecosystem2026-05-02 收录
数据链接:
官方服务:

资源简介:

Title of dataset: Data for "High-temperature low-cycle fatigue and fatigue-creep behaviour of Inconel 718 superalloy: Damage and deformation mechanisms"Name/institution/contact information: Dr. Michal Bartošák, Czech Technical University in Prague - Faculty of Mechanical Engineering, email: michal.bartosak@fs.cvut.czDate of data collection: The data were collected from the start of 2021 to the end of 2023.File name structure: The data within the folder "SEM" are images of microstructural observations of selected specimens. The data within the folder "FATIGUE_LIFE" include the fatigue lifetimes, as well as the stress and strain amplitudes at mid-life, of all investigated specimens. See https://doi.org/10.1016/j.ijfatigue.2024.108369 for the associated article and a detailed description of the methods.

创建时间:
2024-10-17
二维码
社区交流群
二维码
科研交流群
商业服务