AMI - Spatial Atomic Layer Deposition of Molybdenum Oxide for Industrial Solar Cells

收藏
Figshare2020-11-24 更新2026-04-28 收录
官方服务:

资源简介:

Data from each of the figures of:Gregory, G., Luderer, C., Ali, H., Sakthivel, T. S., Jurca, T., Bivour, M., Seal, S., Davis, K. O., Spatial Atomic Layer Deposition of Molybdenum Oxide for Industrial Solar Cells. Adv. Mater. Interfaces 2020, 7, 2000895.