Data for "Emergent B2 chemical orderings in the AlTiVNb and AlTiCrMo refractory high-entropy superalloys studied via first principles theory and atomistic simulations"

收藏
NIAID Data Ecosystem2026-05-02 收录
下载链接:
https://zenodo.org/record/14849314
下载链接
链接失效反馈
官方服务:
资源简介:
Dataset associated with the arXiv preprint "Emergent B2 chemical orderings in the AlTiVNb and AlTiCrMo refractory high-entropy superalloys studied via first principles theory and atomistic simulations" The file 00_README.md explains the file structure of the dataset.