Dateset- Microstructural evolution and mechanical response of ion-irradiated Fe-9Cr alloys: Insights from nanoindentation

收藏
Zenodo2026-04-22 更新2026-05-26 收录
官方服务:

资源简介:

Title: Microstructrual Evolution and mechanical response of ion-irradiated Fe-9Cr alloys: Insights from nanoindentation Authors: K. Mulewska, D. Kalita, M. Wilczopolska, W. Chromiński, P.A. Ferreiros, Ł. Kurpaska Corresponding Author: Katarzyna Mulewska, Orcid: 0000-0001-6863-9431 This record contains files generated in the preparation process of the following publication:Microstructrual Evolution and mechanical response of ion-irradiated Fe-9Cr alloys: Insights from nanoindentation Authors: K. Mulewska, D. Kalita, M. Wilczopolska, W. Chromiński, P.A. Ferreiros, Ł. Kurpaska submitted to Journal of Nuclear Materials (Elsevier) Funding / Project information This dataset is associated with the project funded by the National Science Centre, Poland (NCN):Project number: 2023/49/N/ST11/01257Funding scheme: PRELUDIUM 22 Additional support: Helmholtz-Zentrum Dresden-Rossendorf (RADIATE proposal no. 22003083-ST) Foundation for Polish Science (MAB PLUS/2018/8) Ministry of Science and Higher Education (MEiN/2023/DIR/3795) European Union Horizon 2020 (Grant Agreement No. 857470, NOMATEN Centre of Excellence)

提供机构:
Zenodo
创建时间:
2026-03-19
二维码
社区交流群
二维码
科研交流群
商业服务