Mechanical properties of single V2O5 nanocrystal - nanoindentation measurement in control of the max-load

收藏
DataCite Commons2026-03-26 更新2025-04-16 收录
官方服务:

资源简介:

The DataSet contains the nanoindentation curves (indentation force Fn vs penetrationPd) for a single V2O5 nanocrystal supported on a substrate. The measurements were performed in control of the maximum load of Berkovich indenter force from 2 to 50 mN. Nanoindentation curves were collected on a Nanoidenter TTX-NHT2 CSM. The details about measurements are included in each .text file.

创建时间:
2021-06-20