Small punch creep test data for P92 ar material at 600 °C and a load of 450 N
收藏data.europa2024-06-27 收录
官方服务:
资源简介:
Small punch tensile and creep data obtained in a round robin exercise for the elaboration of an EN standard on small punch testing. Creep tests were carried out at temperatures in the range 550-650 ºC.
本数据集包含为编制小冲杆试验(small punch testing)相关欧洲标准(EN,European Standard)所开展的循环比对试验中获取的小冲杆拉伸与蠕变数据。所有蠕变试验均在550~650摄氏度的温度区间内完成。