Superalloy database: strength and microstructure

收藏
DataCite Commons2024-12-17 更新2024-08-25 收录
官方服务:

资源简介:

Data overview ............. alloy_spreadsheet_v3.1.csv A comma delimited csv file containing the processed superalloy database. The spreadsheet was originally compiled in Google Sheets, with pre-processing carried out using the Google Apps Script. Each row corresponds to a unique alloy, with uniqueness determined by both composition and heat treatments. Each row (alloy) has been assigned a unique tag in the 1st column. Note that constituent alloy phases have their own rows---this is premised on the assumption that the constituent phases are themselves valid equilibrium alloys. alloy_spreadsheet_v3.1_input.csv Similar to alloy_spreadsheet_v3.1.csv, this spreadsheet contains the unprocessed data. alloy_images Contains .png files of alloy microstructure (principally SEM or TEM micrographs). The files are labelled systematically and each name corresponds to a relevant data entry in alloy_spreadsheet_v3.1.csv. Methodological information .......................... The databse has been compiled from a mixture of published scientific articles and commercial or industry datasets. Each data source is cited in the dataset, including a DOI were appropriate. Some data was obtained from plots or figures using the WebPlotDigitizer tool. Data-specific information ......................... Units used in the data are specified in the dataset's header. A dash "-" indicates that a certain element or heat treatment was not used in that particular alloy. An empty entry (cell) indicates that data was missing or simply not collected in the original data source.

创建时间:
2022-12-21
二维码
社区交流群
二维码
科研交流群
商业服务