Uniaxial creep test data for AISI 316L ar material at 650 °C and a stress of 190 MPa (specimen identifier GD-01)

收藏
DataCite Commons2024-10-15 更新2025-04-16 收录
官方服务:

资源简介:

Data created at JRC, Netherlands during the Horizon 2020 NUCOBAM project aiming to develop the qualification process and evaluate the in-service behaviour of AM materials, allowing the use of additively manufactured components in nuclear installations. The project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 945313.