Influence of ruthenium in a model Co-Al-W superalloy
收藏DataCite Commons2024-02-26 更新2024-07-13 收录
下载链接:
https://www.materialsdatafacility.org/detail/pub_6_sauza_influence_v1.2
下载链接
链接失效反馈官方服务:
资源简介:
The effect of 2 at.% Ru addition on a base Co-8.8Al-7.3W at.% superalloy, consisting of a gamma-(fcc) matrix with gamma’-(L12 structure) precipitates is studied
using atom-probe tomography. Ru is found to partition to the gamma' precipitate after aging at 900C for 16h.