遇见数据集

Uniaxial creep test data for ER 316L sa wm material at 600 °C and a stress of 292 MPa (specimen identifier 36819)

收藏
DataCite Commons2023-08-30 更新2025-04-16 收录
官方服务:

资源简介:

Data created by ENEA, Italy during the Horizon 2020 GEMMA project on GenIV materials maturity, including test results from an SSRT round-robin on EUROTRANS/DEMETRA T91 in Pb at 400°C. This project has received funding from the Euratom research and training programme 2014-2018 under Grant Agreement No. 755269.

创建时间:
2022-06-08