five

Battery Degradation Dataset - Li Plating And SEI Growth

收藏
NIAID Data Ecosystem2026-05-02 收录
下载链接:
https://data.mendeley.com/datasets/m8w8sjk3vm
下载链接
链接失效反馈
官方服务:
资源简介:
45 commercial Li−ion coin cells (LIR2025H produced by EEMB Battery) with nickel manganese cobalt oxide (NMC) cathodes and graphite anodes are cycled on a Landt CT3001A battery test system to generate cycle data. The cells are charged under CCCV profile with constant current range from 0.2C to 5.5C. The cutoff voltage ranges from 4.2V to 4.4V. All cells are discharged with C/5. The detail charging profile can be found in the charging policy.xlsx. If you make use of our data, please cite our dataset directly using its DOI, as well as the following papers: Yao, J., Gao, Q., Gao, T., Jiang, B., & Powell, K. M. (2024). A Physics–Guided Machine Learning Approach for Capacity Fading Mechanism Detection and Fading Rate Prediction Using Early Cycle Data. Batteries, 10(8), 283. Please also consider citing our papers on these topics, see: Yao, J., Powell, K., & Gao, T. (2022). A two-stage deep learning framework for early-stage lifetime prediction for lithium-ion batteries with consideration of features from multiple cycles. Frontiers in Energy Research, 10, 1059126.
创建时间:
2024-08-13
5,000+
优质数据集
54 个
任务类型
进入经典数据集
二维码
社区交流群

面向社区/商业的数据集话题

二维码
科研交流群

面向高校/科研机构的开源数据集话题

数据驱动未来

携手共赢发展

商业合作