Dataset to: Heat treatment design for additively manufactured nickel superalloy via Bayesian optimization of ultimate tensile strength and energy consumption

收藏
Zenodo2026-06-22 更新2026-06-12 收录
官方服务:

资源简介:

Dataset to "Katary, E., Sekuła, K., Krok, D., Posmyk, M., Dusza, M., Matusik, W., & Gruber, K. (2026). Heat treatment design for additively manufactured nickel superalloy via Bayesian optimization of ultimate tensile strength and energy consumption. Virtual and Physical Prototyping, 21(1). https://doi.org/10.1080/17452759.2026.2686064" Dataset covers structured folders sorted by data and experiment type, with raw data and processed results supporting all claims in the cited article. Please cite the main paper as well when using this dataset. @article{am-ht-mobo_2026, author = {E. Katary, K. Sekuła, D. Krok, M. Posmyk, M. Dusza, W. Matusik, K. Gruber}, title = {Heat treatment design for additively manufactured nickel superalloy via Bayesian optimization of ultimate tensile strength and energy consumption}, journal = {Virtual and Physical Prototyping}, year = {2026},volume = {21},number = {1},pages = {e2686064}, publisher = {Taylor \& Francis}, doi = {https://doi.org/10.1080/17452759.2026.2686064},} Dataset file description table Main folder Subfolders/Files Description 10_MOBO_exp_PIP seed.csv; experiment_PIP.csv;readme.txt Seed data and full MOBO experiment log for PIP, including process parameters and tensile outputs. 11_MOBO_exp_Hardness seed.csv; experiment_Hardness.csv; readme.txt Seed data and MOBO experiment log for hardness optimization, with heat-treatment parameters and hardness results. 20_EBSD_exp_PIP_PF EBSD_AB_sample/; EBSD_PF_samples/; readme.txt EBSD-derived text data and maps for AB reference and PF samples after PIP processing. 30_SEM_exp_PIP_PF XY/; XZ/; readme.txt SEM images for PIP PF samples, organized by plane (XY/XZ) and PF sample. 31_SEM_exp_Hardness_PF PF01/; PF03/; PF07/; readme.txt SEM images for hardness PF samples, organized by PF sample. 40_OM_exp_PIP_PF PF04/; PF07/; PF08/; PF09/; PF12/; AB/; readme.txt Optical microscopy images for PIP PF samples and AB reference, organized by PF sample and plane. 41_OM_exp_Hardness_PF PF01/; PF03/; PF07/; readme.txt Optical microscopy images for hardness PF samples, organized by PF sample and plane. 50_Tensile_exp_PIP_PF Tensile_exp_PIP_PF_RawData/;Tensile_exp_PIP_PF_Results.csv; Hardness_of_PF_in_exp_PIP.xlsx; readme.txt Raw and processed tensile results for PIP PF samples, plus hardness summary. 51_Tensile_exp_Hardness_PF PF01_exp_Hardness_tensile_RawData/; PF03_exp_Hardness_tensile_RawData/; PF07_exp_Hardness_tensile_RawData/; PF01/03/07_exp_Hardness_tensile_Results.csv; readme.txt Raw and processed tensile results for hardness PF samples.

提供机构:
Zenodo
创建时间:
2026-06-09
二维码
社区交流群
二维码
科研交流群
商业服务