A Quantifiable and Automated Volume Fraction Characterization Technique for Secondary and Tertiary γʹ Precipitates in Ni-based Superalloys
收藏NIAID Data Ecosystem2026-03-10 收录
官方服务:
资源简介:
This is the MIPAR recipe used to segment the gamma prime precipitates from the gamma matrix in the attached SEM image.
创建时间:
2018-02-14