遇见数据集

Uniaxial creep test data for P91 ar material at 650 °C and a stress of 100 MPa (specimen identifier T11359)

收藏
DataCite Commons2023-10-20 更新2025-04-16 收录
官方服务:

资源简介:

Uniaxial creep rupture and creep-fatigue tests have been performed using P91 material in a variety of conditions (ex-service parent metal, new parent metal and ex-service cross-weld specimens). All tests were performed at constant temperature, using machines located at the Australian Nuclear Science and Technology Organisation (ANSTO).

创建时间:
2015-04-20