Shrinkage results data of high-limestone filler concretes
收藏Mendeley Data2026-04-18 收录
下载链接:
https://data.mendeley.com/datasets/d828k98rrk
下载链接
链接失效反馈官方服务:
资源简介:
Free shrinkage test results up to 6 months, according to the NF P 15-433 standard, for three types of PCC formulated with limestone crushed sand rich in fillers (<75µm) as fine aggregates, devoid of superplasticizers.
创建时间:
2023-03-16