Data bundle for "Quantitative precipitate classification and grain boundary property control in Co/Ni-base superalloys"
收藏数据链接:
官方服务:
资源简介:
Data bundle for "Quantitative precipitate classification and grain boundary property control in Co/Ni-base superalloys". Contains correlative EBSD and EDS measurements of alloy microstructures, as well as ThermoCalc simulations. As detailed in https://arxiv.org/abs/2009.00948.