This data publication is based on the metadata and datasets underlying the manuscript: Atomic Layer Deposition on Spray-dried Supraparticles to Rationally Design Catalysts with Ultralow Noble Metal Loadings. The controlled assembly of supraparticles using spray-drying enables the synthesis of nanoporous materials. Changing the size of the constituent nanoparticles or their agglomeration states provides access to a diverse range of pore frameworks. This turns supraparticles into ideal scaffolds in heterogeneous catalysis. The combination of supraparticles with atomic layer deposition (ALD) as a surface functionalization technique offers excellent control over the deposition of a functional material and its distribution over the scaffold on the nanoscale. This work reports the combination of SiO2 supraparticles as tunable scaffolds and their loading with a platinum-based ALD catalyst. The deliberate adjustment of the scaffold pore framework via spray-drying and its effects on the catalyst deposition are highlighted. Furthermore, varying numbers of Pt ALD cycles are applied to explore the capability of the combinational approach with respect to catalyst loading and Pt efficiency. High-resolution electron microscopy reveals ultra-small Pt clusters deposited on the supraparticles after the very first ALD cycle. Using the hydrogenation of 4-nitrophenol as a demonstration, the impact of the pore framework and the Pt deposition variation in ALD on the catalytic functionality is investigated.

提供机构:
Zenodo
创建时间:
2025-04-04
二维码
社区交流群
二维码
科研交流群
商业服务