Data for: Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten
收藏NIAID Data Ecosystem2026-03-11 收录
官方服务:
资源简介:
Nanoindentation test result data obtained from the MD simulation of indentation of tungsten as specified in the manuscript titled "Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten"