Quartz and calcite slide-hold-slide data from dual-axis nanoindenter
收藏NIAID Data Ecosystem2026-05-01 收录
下载链接:
https://zenodo.org/record/8132909
下载链接
链接失效反馈官方服务:
资源简介:
Data from slide-hold-slide experiments performed by a dual-axis nanoindenter (with a diamond Berkovich-type tip) on single crystals of quartz and calcite. The data is in Python's pickle format ("*.pkl") and can be accessed with the pickle library.
创建时间:
2023-10-07