Data for Publication "Nucleation behavior of SnS2 on thiol functionalized SAMs during solution based atomic layer deposition"

收藏
Zenodo2024-07-03 更新2026-05-26 收录
官方服务:

资源简介:

Raw data, reduced data and fitting scripts used to produce figures in publication "Nucleation behavior of SnS2 on thiol functionalized SAMs dur-ing solution based atomic layer deposition", K.Götz et al. in Advanced Materials Interfaces (Wiley), https://doi.org/10.1002/admi.202300990. The data is composed in a .zip file. The zip file contains a folder for each graphic in the publication containing data. In these folders data is filed as "raw data", "reduced data" and "fit script". With the datasets and fit files contained within the .zip folder all data from the publication can be reproduced. The rawdata folders contain the raw data as produced from the used instrument. This consists of: DESY: Detector tiff images for each scattering angle GIWAXS: Detector tiff images, containing silver behenate measurements for distance calibration. XRR Inhouse: xy-ASCII files in .ras format of RIGAKU. AFM: .tiff image produced by PARKS Systems The reduced data contains xy-ASCII files of the data reduced to the form presented in the publication. Fit scripts contain the scripts used to fit the data. This consists of: .hgx files for genX for XRR fits a file structure with scripts to use with the DISCUS suite for the GIWAXS data

提供机构:
Zenodo
创建时间:
2024-07-03
二维码
社区交流群
二维码
科研交流群
商业服务