Investigation of crack nucleation in superalloys using advanced neutron methods
收藏B2FIND2026-04-25 收录
官方服务:
资源简介:
It is proposed that crack nucleation will be investigated at ISIS using the EnginX beam line with the IMAT imaging detector. Notched LCF specimens with varying materials and Kt...