Uniaxial creep test data for ALLOY 800HT material at 850 °C and a stress of 40 MPa
收藏官方服务:
资源简介:
Uniaxial creep data for ALLOY 800HT material from tests performed at Babcock Energy Limited (now Doosan Babcock) in the first-phase Basic Research for Industrial Technologies in Europe (BRITE) P1209 project on lifetime prediction and extrapolation methodologies for computer aided assessment of component service behaviour under stress at high temperature.
创建时间:
2017-09-13