This is an example dataset for use with AstroEBSD. It is a compressed version of the one found at 10.5281/zenodo.3617455, the data bundle for our paper 'Advancing characterisation with statistics from correlative electron diffraction and X-ray spectroscopy, in the scanning electron microscope' - https://doi.org/10.1016/j.ultramic.2020.112944. The .h5 file contains EBSD patterns and EDS spectra. The zip file contains an example analysis, including EDS spectra quantification in a .xls file, which is required for the EDS post-analysis.