Measurements of thermal conductivity made during Ocean Drilling Program (ODP) Leg 131 were corrected during the cruise using the following set of standards: fresh water, fused silica, Macor ceramic, and basalt. The true thermal conductivity of the basalt standard was not known during Leg 131. In this report, we use a corrected conductivity value for the basalt standard to calibrate measurements made during the leg.