Experimental Validation of Residual Stress FEM Simulation in As-Quenched Superalloy Discs

收藏
NIAID Data Ecosystem2026-03-12 收录
官方服务:

资源简介:

Thermomechanical simulation results were validated by a practical strategy of coupled experimental techniques to reveal in-depth residual stress profiles.