The open-source, python-based SpherIndent software package [https://doi.org/10.18434/mds2-4080] developed at NIST provides functionalities spanning from experiment calibration, to experiment analysis, to data extraction and visualization of data collected for spherical nanoindentation experiments. Capabilities and usage of SpherIndent software package have been described in [paper citation]. For reference and training purposes, this data publication provides users interested in SpherIndent with the demonstration datasets referred to in the software paper.