Feasibility tests for DCT and PCT in Ni718 superalloy
收藏官方服务:
资源简介:
A new batch of samples with different grain sizes (20 - 100 µm) and different precipitation states has been delivered for the upcoming InnovXN project. We will assess the suitability of these samples for DCT. The presence of micrometer sized precipitates in this alloy should allow using Digital Volume Correlation (DVC) for assessing the strain fields.