Phase and diffraction contrast tomography of slip localization in In718 superalloy
收藏官方服务:
资源简介:
Phase and diffraction contrast tomography of slip localization in In718 superalloy
创建时间:
2024-12-03

Phase and diffraction contrast tomography of slip localization in In718 superalloy