Corrosivity Caused by Salt Solutions Employed in the Wood Dimensional Stability
收藏DataCite Commons2021-03-23 更新2024-07-25 收录
下载链接:
https://scielo.figshare.com/articles/dataset/Corrosivity_Caused_by_Salt_Solutions_Employed_in_the_Wood_Dimensional_Stability/5670337/1
下载链接
链接失效反馈官方服务:
资源简介:
ABSTRACT The study aimed to evaluate the corrosivity of salt solutions after and before the impregnation in the wood. Solutions with concentration of 5% of chloride of lithium, sodium carbonate, magnesium sulphate, zinc sulphate and copper sulphate II had been kept during 6 hours, at 25; 45 and 100 °C, in contact with steel plates carbon samples of 1.25 × 0.1 × 7.5 cm (width × thickness × length), before and after its contact with wood samples of Corymbia torelliana and Eucalyptus cloeziana. There was no effect of the temperature in the corrosion of the pure solutions. After the contact with woods, corrosivity was incremented with copper II and zinc sulphate solutions. Copper II sulphate caused the biggest loss of mass in plates, and its contact with metallic surfaces is not recommended as wood treatment and drying chambers.
提供机构:
SciELO journals
创建时间:
2017-12-05