Precious metal catalysts are crucial in industrial catalytic processes but are often limited by their scarcity and toxicity. In response, our study explores nickel-based catalysts synthesized using liquid-phase atomic layer deposition (L-ALD), an innovative method developed in our lab that allows precise control over metal dispersion at the atomic scale. We propose to use operando XAS techniques to investigate two novel catalysts: (1) nickel supported on MgO-Al₂O₃ for the dry reforming of methane (DRM), aiming to enhance selectivity toward either CO or H₂, and (2) nickel confined within the mesoporous structure of Al-MCM-41 for low-temperature hydrogenolysis of lignin.