five

Data for "Investigation of local strain rate sensitivity in dual-phase Ti alloys by nanoindentation"

收藏
Mendeley Data2024-03-27 更新2024-06-27 收录
下载链接:
https://zenodo.org/record/32145
下载链接
链接失效反馈
官方服务:
资源简介:
Data for "Investigation of local strain rate sensitivity in dual-phaes Ti alloys by nanoindentation" Tea-Sung Jun1, David E.J. Armstrong2 and T. Benjamin Britton1 1. Department of Materials, Imperial College London, Prince consort Road, London, SW7 2AZ, UK 2. Department of Materials, University of Oxford, Parks Road, Oxford, OX1 3PH, UK -- This nanoindentation data folder contains 3 subfolders: (1) Raw indentation data obtained from TestWorks (2) Data for Figure 4 (3) Data for Figure 5 -- In the subfolder (1), each file name indicates Material_Grain orientation_Indentation strain rate (e.g. 6242_H_0001). For the subfolders (2) and (3), readers can plot the graphs either using Excel, OriginPro or other software. Note that we used the OriginPro to generate all the graphs in this article. -- If readers need further information, please feel free to contact: t.jun@imperial.ac.uk or terryjun83@gmail.com (Tea-Sung (Terry) Jun)
创建时间:
2023-06-28
二维码
社区交流群
二维码
科研交流群
商业服务