Data for: Evaluation of the elastic-plastic properties of TiN coating by nanoindentation technologies using FEM-reverse algorithm
收藏Mendeley Data2021-01-15 更新2026-04-09 收录
下载链接:
https://data.mendeley.com/datasets/2nvpx6h2s2
下载链接
链接失效反馈官方服务:
资源简介:
Research on the elasto-plastic properties of the coating using the reverse analysis method
创建时间:
2021-01-15