Uniaxial creep test data for X10CrMoVNb9 1 / X20CrMoV12 1 - dj material at 600 °C and a stress of 46 MPa (second repeat test)

收藏
DataCite Commons2020-10-10 更新2025-04-16 收录
官方服务:

资源简介:

Data generated in the scope of a project to investigate the influence of weld strength reduction on long-term integrity of power plant components made from heat-resistant martensitic steels.