Raw data of nanoindentation and micro scratch tests on brittle materials
收藏NIAID Data Ecosystem2026-03-10 收录
下载链接:
https://data.mendeley.com/datasets/m46hwp78h4
下载链接
链接失效反馈官方服务:
资源简介:
It is the raw data of nanoindentation and micro scratch tests on brittle materials such as borofloat 33 glass, soda-lime glass, granite, boron carbide (B4C), aluminium oxide (Al2O3) and silicon carbide (SiC).
创建时间:
2018-04-09