Experimental data related to the publication: "Radiofrequency plasma spheroidization of complex concentrated superalloy Al10Nb20Ta15Ti30V5Zr20 "
收藏官方服务:
资源简介:
SEM micrographs Figures 1 and 2: raw *.tiff files with metadata in the TIFF tags within the files EDS measurements Tab5_eds_sem.h5 contains the SEM EDS measurements presented in Table 4. Metadata are included within the file. XRD data Figure 3: *.raw binary files with experimental 1D diffraction patterns (metadata included) TEM micrographs Figures 4 and 5: raw *.dm4 files, can be opened by e.g. ImageJ/Fiji suite Figure 5d: STEM micrograph with metadata as a separate file APT data Figure 6: raw *.HITS file with metadata included, to be opened in e.g. IVAS suite