The role of grain boundaries in low-temperature plasticity of olivine revealed by nanoindentation

收藏
Figshare2022-11-07 更新2026-04-08 收录
下载链接:
https://figshare.com/articles/dataset/The_role_of_grain_boundaries_in_low-temperature_plasticity_of_olivine_revealed_by_nanoindentation/21507060/2
下载链接
链接失效反馈
官方服务:
资源简介:
Nanoindentation, HR-EBSD and TEM data published in the manuscript titled <em>The role of grain boundaries in low-temperature plasticity of olivine revealed by nanoindentation. </em>The pre-print version of the manuscript can be found at: https://doi.org/10.1002/essoar.10512783.1
提供机构:
Wallis, David J; Avadanii, Diana; Marquardt, Katharina; Wilkinson, Angus J.; Hansen, Lars; ohl, markus