The role of grain boundaries in low-temperature plasticity of olivine revealed by nanoindentation
收藏数据链接:
官方服务:
资源简介:
Nanoindentation, HR-EBSD and TEM data published in the manuscript titled <em>The role of grain boundaries in low-temperature plasticity of olivine revealed by nanoindentation. </em>The pre-print version of the manuscript can be found at: https://doi.org/10.1002/essoar.10512783.1