Supplementary Data and Codes for "An Active Learning Framework for the Rapid Assessment of Galvanic Corrosion"
收藏官方服务:
资源简介:
This dataset contains the supplementary data and supporting information for the manuscript "An Active Learning Framework for the Rapid Assessment of Galvanic Corrosion" , which has been submitted to npj Materials Degradation. The .zip file has a README that outlines the structure of the dataset and the contents of all the folders therein. Please direct further queries to Aditya Venkatraman - avenkat@sandia.gov