BAM Reference Data: Creep of Single-Crystal Ni-Based Superalloy CMSX-6

收藏
Zenodo2025-01-28 更新2026-05-26 收录
官方服务:

资源简介:

This publication provides comprehensive metadata and test results of constant force creep tests according to DIN EN ISO 204:2019-4 on the single crystal Ni-based superalloy CMSX-6 at T = 980 °C and initial stressesbetween 140 MPa and 230 MPa. The tests were carried out in an accredited test laboratory using calibrated measuring equipment. The data were audited and are BAM reference data.