<b>High throughput analysis of protein adsorption to a large library of polymers using liquid extraction surface analysis – tandem mass spectrometry (LESA-MS/MS)</b>
收藏NIAID Data Ecosystem2026-05-02 收录
数据链接:
官方服务:
资源简介:
Raw data for optimisation of LESA-MS/MS parameters for the analysis of in situ digests on synthetic polymer substrates. Raw LESA-MS/MS for screening a library of homopolymers for investigation of protein-material interaction.ToF-SIMS data for quality assesment of printing and polymerizationBrightfield images of polymer arrays
创建时间:
2025-06-03