In situ nanotomography investigation of cavity growth during high temperature deformation
高温变形过程中孔洞生长的原位纳米断层扫描(in situ nanotomography)研究
应用场景:
相关数据集
Processed data-Dynamic softening behavior of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting microstructure during hot deformation
The processed data includes strain-rate sensitivity exponent, deformation activation energy, power dissipation distribution and Poliak-Jonas criterion of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy correspond
Mendeley Data2024-01-31 更新80
The identification of dynamic softening behavior and constitutive modeling during hot deformation of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting microstructure
The true stress-strain data of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting structure obtained by carrying a series of isothermal compression tests at temperatures of 940-1030℃ and strai
Mendeley Data2024-03-27 更新50
Recrystallization Kinetics of Fe-3%Si after Deformation at High Strain Rate and High Temperature
Recrystallization kinetics of Fe-3%Si with initial grain size 296~839µm at the temperature range 1223~1423K, strain range from 0.51 to 0.92, strain rate range 5~80s−1 was studied by isothermal compres
DataCite Commons2020-08-26 更新40
The identification of dynamic softening behavior and constitutive modeling during hot deformation of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting microstructure
The true stress-strain data of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting structure obtained by carrying a series of isothermal compression tests at temperatures of 940-1030℃ and strai
NIAID Data Ecosystem60
Dynamic softening behavior of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting microstructure during hot deformation
The true stress-strain data of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si alloy with lamellar starting structure obtained by carrying a series of isothermal compression tests at temperatures of 850-1030℃ and strai