Enhanced strength-ductility and stress-rupture properties of a Ni-based superalloy via nanotwins and stable γ’ particles

收藏
DataCite Commons2026-04-24 更新2026-05-03 收录
下载链接:
https://tandf.figshare.com/articles/dataset/Enhanced_strength-ductility_and_stress-rupture_properties_of_a_Ni-based_superalloy_via_nanotwins_and_stable_particles/30824076/1
下载链接
链接失效反馈
官方服务:
资源简介:
Here, we alter the alloying elements of GH4742 superalloy by means of domain-knowledge informed thermodynamic calculation to reduce the stacking fault energy of the γ matrix and enhance the stability of γ’ particles. Increasing Co and Cr concentrations with Mo substitution by W induces the formation of high-density stacking faults and nanotwins, while reducing the coarsening rate of γ’ particles during tensile testing at 760°C and stress-rupture loading at 760°C/480 MPa. Thus, the yield strength, working-hardening capacity, and stress-rupture life are simultaneously improved, achieving the synergic enhancements in strengths-ductility and stress-rupture properties at elevated temperature.
提供机构:
Taylor & Francis
创建时间:
2025-12-08
二维码
社区交流群
二维码
科研交流群
商业服务