遇见数据集

nanoindentation data associated with the publication "On the elastic microstructure of bulk metallic glasses" in Materials&Design 2023

收藏
Zenodo2024-07-09 更新2026-05-26 收录
官方服务:

资源简介:

This dataset consists of indentation data measured with a conospherical tip in a Hysitron-Bruker TI980 Nanoindenter on the surface of a <100> Silicon wafer and a polished cross-sectional cut of a Zr65Cu25Al10 bulk metallic glass. It is associated with the following publication: Birte Riechers, Catherine Ott, Saurabh Mohan Das, Christian H. Liebscher, Konrad Samwer, Peter M. Derlet and Robert Maass "On the elastic microstructure of bulk metallic glasses" Materials and Design 229, (2023) 111929. https://doi.org/10.1016/j.matdes.2023.111929 All experimental information can be found in this paper and in the accompanying supplementary information. This electronic version of the data was published on the "Zenodo Data repository" found at http://zenodo.org/deposit in the community "Bundesanstalt fuer Materialforschung und -pruefung (BAM)". The authors have copyright to these data. You are welcome to use the data for further analysis, but are requested to cite the original publication whenever use is made of the data in publications, presentations, etc. Any questions regarding the data can be addressed to birte.riechers@bam.de who would also appreciate a note if you find the data useful. ____________________________________________________________________ The data format is defined as described below: In total, Fifteen text files exist that result in five different data sets. Two data sets represent measurements on Silicon, these are specifically the topography (mapped height profile) and indentation modulus (Si-topography.txt and Si-modulus.txt). The connected lateral information of these mapped quantities (i.e. Si-X_topography.txt and Si-Y_topography.txt; Si-X_modulus.txt and Si-Y_modulus.txt). This amounts to six .txt files connected to measurements on Silicon. Three data sets represent measurements on the Zr65Cu25Al10 bulk metallic glass. These are specifically the topography (MG-topography.txt), the indentation modulus (MG-modulus.txt), and the curvature-corrected indentation modulus (MG-curvcorr_modulus.txt). The connected lateral information of these mapped quantities (i.e. MG-X_topography.txt and MG-Y_topography.txt; MG-X_modulus.txt and MG-Y_modulus.txt; MG-X_curvcorr-modulus.txt and MG-Y_curvcorr-modulus.txt). This amounts to nine .txt files connected to measurements on the metallic glass. The files are plain text files with the data points separated by commata. Topography data is stated in units of Nanometer, modulus data is stated relative to its mean as unit-less values. Beside the .txt files, one figure (.pdf) with a plot of each data set is provided for reference, and the python code (Riechers_OnTheElasticMicrostructureOfBulkMetallicGlasses_zenodo.ipynb) generating these figures from the data sets is uploaded to this repository as well.

提供机构:
Zenodo
创建时间:
2023-04-12
二维码
社区交流群
二维码
科研交流群
商业服务