High throughput analysis of protein adsorption to a large library of polymers using liquid extraction surface analysis – tandem mass spectrometry (LESA-MS/MS)

收藏
Figshare2025-06-03 更新2026-04-28 收录
官方服务:

资源简介:

Raw data for optimisation of LESA-MS/MS parameters for the analysis of in situ digests on synthetic polymer substrates. Raw LESA-MS/MS for screening a library of homopolymers for investigation of protein-material interaction.ToF-SIMS data for quality assesment of printing and polymerizationBrightfield images of polymer arrays