Dataset in numerical simulation of laser welding of nickel-based superalloy
收藏科学数据银行2022-11-08 更新2026-04-23 收录
下载链接:
https://www.scidb.cn/detail?dataSetId=df6f5b12bccf451daa946a16771955e2
下载链接
链接失效反馈官方服务:
资源简介:
the result in the thermal cycle, the evolution law of thermal stress-strain and the mechanical mechanism of the fiber laser welding and CO2 laser welded superalloy Inconel 617
提供机构: