Comparisson of area specific resistance of the SrTi1-xFexO3-d porous oxygen electrodes and state-of-the-art LSCF sintered at optimal conditions
收藏Mendeley Data2024-01-31 更新2024-06-30 收录
下载链接:
https://mostwiedzy.pl/en/open-research-data/comparisson-of-area-specific-resistance-of-the-srti1-xfexo3-d-porous-oxygen-electrodes-and-state-of-the-art-lscf-sintered-at-optimal-conditions,52310590555771-0
下载链接
链接失效反馈官方服务:
资源简介:
In this dataset are presented results of the polarization resistance of optimaly sintered SrTi1-xFexO3-d porous oxygen electrodes in symetrical cell (1000 °C; 800 °C and 800°C respectively x = 0.35; 0.50 and 0.70). For commparison were selected commercially avilable state-of-the-art LSCF (Europa) sintered at 1050 °C. The measurement temperature range was between 800 °C and 500 °C in syntetic air (40 ml min-1 flow). Results converted to electrode surfaces area and dived by two electrodes.
创建时间: