Deformation mechanisms of a newly developed Ni-base superalloy at cryogenic t...
收藏B2FIND2026-04-25 收录
下载链接:
https://b2find.eudat.eu/dataset/7d85cbd1-2a1c-5f75-aeda-172298a1f650
下载链接
链接失效反馈官方服务:
资源简介:
Haynes 282 is a novel Ni-base superalloy, combining excellent weldability and general processability with moderate cost. As such, it is very promising for e.g. industrial gas...