Using nanoindentation to quantify the mechanical profile of Wufeng-Longmaxi formation shale in Southwest China: Link to sedimentary conditions
收藏Mendeley Data2026-04-09 收录
下载链接:
https://data.mendeley.com/datasets/w9cd2tbss5
下载链接
链接失效反馈官方服务:
资源简介:
The data for "Using nanoindentation to quantify the mechanical profile of Wufeng-Longmaxi formation shale in Southwest China: Link to sedimentary conditions".